Symmetry

How is the symmetry determined?

The symmetry of each MOF is determined using Pymatgen's SpacegroupAnalyzer with a symprec tolerance of 0.1. The symmetry is based on the PBE-D3(BJ) optimized structure. It should be noted that all structure relaxations were carried out without explicit symmetry constraints of any kind.